Brand Name: Global
Model Number: AFB-102
Place of Origin: Zhejiang, China (Mainland)
When heated,this silver brazing flux spreads quickly and wets the surface completely .alloys will also flow better.Protects from discoloration of the braze area. Remove excess flux by hot water rise .To thin ,add small amount of water and styr until flux creamy.keep lid tightly closed.
Flux No. |
Ingredient |
From |
Application |
AFB-102 |
Fluorine boric potassium four boric acid potassium,bric acid and so on. |
powder |
Use with silver-bearing alloys jointing copper-copper, steel-stainless steel and dissimilar metals. Active Range 600-850°C |
AFB-102 |
Fluorine boric potassium four boric acid potassium,bric acid and so on |
paste |
|
AFB-103 |
Fluorine boric acid potassium, potassium carbonate and so on. |
powder |
|
AFB-204 |
KF-ALF3 |
powder |
Use with Aluminum-silicon alloys for brazing of pure Alu-Alu,Alu-Manganese alloy. Active range 560-620°C |